French nuclear regulator approves EDF's next steps in investigating stress corrosion

Jiří Salavec
Jiří Salavec
31 July 2022, 08:20
French nuclear regulator approves EDF's next steps in investigating stress corrosion

Energy company EDF has received approval from the French nuclear regulator for its strategy for analysing and addressing stress corrosion. EDF discovered stress corrosion cracks in welds at some of its nuclear power plants during routine outages. The analyses carried out identified susceptible sections that should be inspected by 2025.

The French nuclear regulator Autorité de Sûreté Nucléaire (ASN) announced that it considers EDF’s strategy for addressing stress corrosion issues appropriate in light of the information obtained so far. Since the problem was discovered at the Civaux nuclear unit at the end of 2021, 12 units in France have been taken offline for detailed analysis.

EDF has so far carried out laboratory analyses of 70 weld samples from a total of 8 nuclear units. The analyses identified susceptible sections of piping that need to be thoroughly inspected. These are the pipes of the safety injection system (RIS - safety injection system) and the suction pipes of the residual heat removal system. EDF plans to inspect all its nuclear units by 2025.

Translation disclaimer

This article is a machine translation of the Czech original and has not yet been fully reviewed. In case of any doubt, please refer to the Czech version.

The article continues for subscribers

Premium content

The rest of this article is available to premium subscribers only. Get access to all premium articles on oEnergetice.cz.

Best value: annual subscription

Monthly option 4 € / month

3.25 €/ month

I already have a subscription